KingflexItilize kawoutchou butyronitrile ak klori polivinil (NBR, PVC) kòm prensipal matyè premyè atravè kimen ak lòt pwosedi espesyal pou fòme materyèl izolasyon chalè ki mou ak pò fèmen. San klorofluorokarbon (CFC) ak fòmaldeyid. Pèfòmans faktè chalè ak konduktivite a te dirab ak estab epi pèfòmans rezistans dife a te pi wo (endis oksijèn ≥40%).
Dimansyon Kingflex | |||||||
Tepesè | Width 1m | Wlongè 1.2m | Wlajè 1.5m | ||||
Pous | mm | Gwosè (L * W) | ㎡/Woule | Gwosè (L * W) | ㎡/Woule | Gwosè (L * W) | ㎡/Woule |
1/4" | 6 | 30 × 1 | 30 | 30 × 1.2 | 36 | 30 × 1.5 | 45 |
3/8" | 10 | 20 × 1 | 20 | 20 × 1.2 | 24 | 20 × 1.5 | 30 |
1/2" | 13 | 15 × 1 | 15 | 15 × 1.2 | 18 | 15 × 1.5 | 22.5 |
3/4" | 19 | 10 × 1 | 10 | 10 × 1.2 | 12 | 10 × 1.5 | 15 |
1" | 25 | 8 × 1 | 8 | 8 × 1.2 | 9.6 | 8 × 1.5 | 12 |
1 1/4" | 32 | 6 × 1 | 6 | 6 × 1.2 | 7.2 | 6 × 1.5 | 9 |
1 1/2" | 40 | 5 × 1 | 5 | 5 × 1.2 | 6 | 5 × 1.5 | 7.5 |
2" | 50 | 4 × 1 | 4 | 4 × 1.2 | 4.8 | 4 × 1.5 | 6 |
Done teknik Kingflex | |||
Pwopriyete | Inite | Valè | Metòd Tès la |
Ranje tanperati | °C | (-50 - 110) | GB/T 17794-1999 |
Ranje dansite | Kilogram/m3 | 45-65Kg/m3 | ASTM D1667 |
Pèmeyabilite vapè dlo | Kg/(mspa) | ≤0.91 × 10﹣¹³ | DIN 52 615 BS 4370 Pati 2 1973 |
μ | - | ≥10000 | |
Konduktivite tèmik | W/(mk) | ≤0.030 (-20°C) | ASTM C518 |
≤0.032 (0°C) | |||
≤0.036 (40°C) | |||
Evalyasyon dife | - | Klas 0 ak Klas 1 | BS 476 Pati 6 pati 7 |
Endèks Pwopagasyon Flanm dife ak Devlopman Lafimen |
| 25/50 | ASTM E 84 |
Endèks Oksijèn |
| ≥36 | GB/T 2406, ISO4589 |
Absòpsyon dlo, % pa volim | % | 20% | ASTM C209 |
Estabilite dimansyon |
| ≤5 | ASTM C534 |
Rezistans chanpiyon | - | Bon | ASTM 21 |
Rezistans ozòn | Bon | GB/T 7762-1987 | |
Rezistans a UV ak move tan | Bon | ASTM G23 |
Avèk pèfòmans ki estab, anti-krak, rezistans a tanperati ki wo ak ba, ak gwo elastisite ak sou sa, ekselan rezistans korozyon fè pwodwi a pa fasil pou vyeyi, pwodwi sa a pratik e senp pou enstale, epi li itilize yon lavi ki long..